纺织学报 ›› 2008, Vol. 29 ›› Issue (6): 85-87.

• 染整与化学品 • 上一篇    下一篇

BTCA免烫织物在洗涤过程中免烫性能的衰变

周敬1;于永玲1;张亚慧2   

  1. 1.大连工业大学纺织轻工学院 辽宁大连116034;2.辽宁出入境检验检疫局 辽宁大连116001
  • 收稿日期:2007-06-26 修回日期:2007-12-25 出版日期:2008-06-15 发布日期:2008-06-15

Deterioration of noniron performance of BTCA finished fabric in wash process

ZHOU Jing;YU Yongling;ZHANG Yahui   

  1. 1.School of Textile and Light Industry;Dalian Polytechnic University;Dalian;Liaoning 116034;China;2.Liaoning Entry-Exit Inspection and Quarantine Bureau;Dalian;Liaoning 116001;China
  • Received:2007-06-26 Revised:2007-12-25 Online:2008-06-15 Published:2008-06-15

摘要: 针对免烫织物免烫功能的持续性问题,通过测试免烫织物折皱回复角,分析研究免烫织物在洗涤过程中免烫性能衰败的过程、机制和规律。研究结果表明:对于BTCA无甲醛免烫整理棉织物,随水洗次数的增加,免烫性能衰变显著;经过干洗后,折皱回复角的变化较小,免烫织物仍然具有较强的免烫性能。

Abstract: Durability of noniron performance of noniron fabric is a long standing problem.The paper investigates the deteriorative process,mechanism and rule of noniron performance of noniron fabric in wash process by measuring and analyzing the wrinkle recovery angle of the fabric.The findings indicate that as to formaldehyde-free BCTA finished noniron cotton fabric,increasing laundering times decreases the noniron performance remarkably;however,after dry-cleaning,the fabric exhibits smaller change in wrinkle recovery angle and retains better noniron performance.