纺织学报 ›› 2006, Vol. 27 ›› Issue (11): 6-9.

• 研究论文 • 上一篇    下一篇

毛条成形中长度损伤的演变与表征:(1)纤维的断裂——显性损伤

于伟东1.2;王华强1.3   

  1. 1.东华大学纺织学院 上海201620;2.武汉科技学院材料与纺织学院 湖北武汉430074;3.上海海关高等专科学校经济系;上海201204
  • 收稿日期:2005-08-26 修回日期:2005-12-14 出版日期:2006-11-15 发布日期:2006-11-15

Characterization and evolvement of fiber-length damage in wool top making:part (1) fiber breaking—explicit damage

YU Wei-dong 1;2;WANG Hua-qiang3   

  1. 1. College of Textile;Donghua University;Shanghai 201620;China; 2. Institute of Textile and Material;Wuhan University of Science and Engineering;Wuhan;Hubei 430074;China;3.Economics Department;Shanghai Customs College;Shanghai 201204;China
  • Received:2005-08-26 Revised:2005-12-14 Online:2006-11-15 Published:2006-11-15

摘要: 在成条加工中纤维长度会损伤或变短,其中纤维的断裂——显性损伤是纤维损伤的基本部分。采用2次从纤维束头端反复制取一端整齐的纤维丛试样(C试样),可获得分析纤维显性损伤的长度特征值。基于长度特征值建立的差异率和损伤率指标,可有效地表征纤维的这类损伤。实测证明毛条加工各工序都有长度损伤,平均值为8.763%,综合等效长度的变短可达86%以上;而较为敏感和稳定的长度表达指标应该取短纤维率和根数加权平均长度。

Abstract: Fiber-length will be damaged and shortened in top-making due to fiber breaking, namely the explicit damage. A one-end uniform staple sample (sample C) is prepared by aligning twice through pulling_out fibers from both ends of the fiber bundle respectively, and length parameters of fiber-length damage can be obtained through analyzing sample C. The difference rate and the damage percentage calculated from the length parameters can be used to characterize fiber-length explicit damage effectively and accurately. The test results verify that the explicit damage takes place in all processing processes of the top with an average damage percentage of 8.763%, and the length shortening of the damaged fiber may reach up to 86% of the original one. Meanwhile, the sensitive and stable parameters to evaluate the damages should be expressed by the average weighted length of the short fiber content (SFC) length and the number of fibers.