纺织学报 ›› 2014, Vol. 35 ›› Issue (9): 19-0.

• 纤维材料 • 上一篇    下一篇

纺粘非织造用聚乳酸/聚(3-羟基丁酸-co-3-羟基戊酸共聚酯)的可纺性

  

  1. 1. 浙江理工大学
    2. 浙江理工大学;教育部先进纺织材料加工及制备技术重点实验室
  • 收稿日期:2013-09-25 修回日期:2014-04-01 出版日期:2014-09-15 发布日期:2014-09-16
  • 通讯作者: 韩建 E-mail:hanjian8@zstu.edu.cn
  • 基金资助:

    国家自然科学基金资助项目;浙江省自然科学基金项目;浙江省科技厅计划项目;“产业用纺织材料技术”浙江省重点科技创新团队项目;“受浙江省高校重中之重学科开放基金资助”

Research on the spinnability of Poly(lactic acid)/ Poly(3-hydroxybutyrate-co-3-hydroxyvalerate) two-component biodegradable materials for spun-bonded nonwovens

朱斐超 1,HAN Jian   

  • Received:2013-09-25 Revised:2014-04-01 Online:2014-09-15 Published:2014-09-16
  • Contact: HAN Jian E-mail:hanjian8@zstu.edu.cn

摘要: 为获得高质量的聚乳酸/聚(3-羟基丁酸-co-3-羟基戊酸共聚酯)(PLA/PHBV)双组份生物降解纺粘非织造材料,对PLA/PHBV母粒的相对分子量及分布、熔体指数、热学、结晶和流变性能进行了研究,并对PLA/PHBV纺粘纤维的热学和结晶性能作出了初步探讨。研究表明:PLA/PHBV母粒重均分子量约为120000,分布指数1.99;热失重起始热分解温度285℃,适宜纺粘非织造挤出加工,合适的纺粘加工温度约为210℃。PLA/PHBV熔体在剪切速率小于1000rad/s时,表观粘度对剪切速率变化敏感;熔体对温度的敏感程度随着剪切速率的增大而降低。纺粘加工工艺对PLA/PHBV原料的热学和结晶性能影响显著,较PLA/PHBV母粒,纺粘纤维结晶度下降明显,但非晶区取向程度提高。

Abstract: In order to obtain high quality of Poly(lactic acid)(PLA)/ Poly(3-hydroxybutyrate-co-3-hydroxyvalerate)(PLA/PHBV) two-component biodegradable spun-bonded nonwovens, the relative molecular weight and distribution, melt flowing index, thermal properties, crystallization and rheological behavior of PLA/PHBV masterbatch were investigated, the thermal properties and crystallization of spun-bonded fiber were also discussed. The results showed that the weight-average molecular weight of PLA/PHBV was about 120000 and molecular weight distribution was 1.99;The initial decomposition temperature was 285 ℃,it was suitable for spun-bonded extrusion processing and the appropriate processing temperature was about 210 ℃. The apparent viscosity of PLA/PHBV melt was sensitive to the shear rate when under 1000 rad/s,but the level of sensitivity to temperature lowered when the shear rate increased. The spun-bonded processing conditions had significant effects on the thermal properties and crystallization of PLA/PHBV masterbatch,compared with masterbatch,the degree of crystallinity of spun-bonded fiber decreased obviously but the orientation in amorphous region increased.

No related articles found!
Viewed
Full text
460
HTML PDF
Just accepted Online first Issue Just accepted Online first Issue
0 0 0 0 0 460

  From Others local
  Times 346 114
  Rate 75% 25%

Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!