摘要:

为提高活性染料传统轧-蒸染色的固色率和染深性,将真空脱水技术引入棉织物活性染料轧-蒸染色过程。研究了棉织物含水率、汽蒸时间和碳酸钠用量对活性金黄SRE湿蒸染色的影响,并比较了活性金黄SRE采用浸轧-真空脱水-湿蒸(P-Vac-S)工艺与传统浸轧-湿蒸(P-S)工艺染色棉织物的染深性和耐摩擦色牢度。结果表明:浸轧含25 g/L活性金黄SRE染液的棉织物,将其含水率真空脱水至20% ~ 30%,再进行湿蒸,染得棉织物的小染率(K/S值)和染料固色率相对较高;含水率为(25 ± 2)%的棉织物湿蒸染色的适宜汽蒸时间和碳酸钠质量浓度分别为5 min和25 g/L;采用活性金黄SRE采用P-Vac-S工艺染色棉织物的K/S值比采用P-S工艺染色的K/S值高15% ~ 30%,但是经前者染色棉织物的耐摩擦色牢度比后者略差。

关键词: 活性金黄SRE, 棉织物, 真空脱水, 湿蒸染色, 染深性

Abstract:

In order to enhance the fixation rate and color build-up property of reactive dyes in the conventional pad-steam (P-S) dyeing process, a vacuum-dewatering  procedure was incorporated. Factors influencing the wet -steaming dyeing of reactive golden yellow SRE, such as the water content of the padded cotton fabric, the steaming time and sodium carbonate dosage were investigated. The color build-up property and rubbing fastness of the cotton fabrics dyed using the pad vacuum-dehydration steam (P-Vac-S) process and the P-S process were compared as well. The results show that cotton fabrics padded with 25 g/L dye liquor exhibited higher K/S value and dye fixation rate by reducing the fabric water content down to 20% ~ 30% by vacuum-dehydration prior to the steaming stage. The steaming time of 5 min and sodium carbonate concentration of 25 g/L were appropriate for dyeing of padded cotton fabrics with (25 ± 2)% water content. The K/S value of the cotton fabric is impeoved by 15% ~ 30% when dyed by the P-Vac-S process, compared with that by the P-S process, however, the rubbing fastness of the cotton fabric obtained by the former process was a bit poorer than that by the later process.

Key words: reactive golden yellow SRE, cotton fabric, vacuum-dewatering, wet-steaming dyeing, color build-up property

中图分类号: 

  • TS 193.5
[1] 肖慧芳 阎克路 纪柏林. 糖类添加剂在1,2,3,4-丁烷四羧酸棉织物防皱整理中的应用[J]. 纺织学报, 2018, 39(07): 89-94.
[2] 黄益 李思琪 阮斐斐 李博 邵建中. 卟啉铁/双氧水体系在棉织物低温催化漂白中的应用[J]. 纺织学报, 2018, 39(06): 75-80.
[3] 舒大武 房宽峻 刘秀明 李新禹 刘曰兴 张健飞 张鑫卿. 织物升温速率对活性染料轧-蒸无盐染色的影响[J]. 纺织学报, 2018, 39(02): 106-111.
[4] 白刚 刘艳春. 触感清凉棉织物的制备及其性能[J]. 纺织学报, 2018, 39(01): 94-97.
[5] 颜东 邓继勇 汪南方 王连军. 有机硅改性聚氨酯/丙烯酸酯共聚乳液对棉织物的抗皱整理[J]. 纺织学报, 2018, 39(01): 89-93.
[6] 邓继勇 柳芊 董新理 汪南方. 新型氮-磷阻燃剂制备及其对棉织物的阻燃性能[J]. 纺织学报, 2017, 38(11): 97-101.
[7] 韩莹莹 孙丽静 钟毅 徐红 毛志平 . 活性染料Pickering乳液非均相浸渍染色[J]. 纺织学报, 2017, 38(11): 79-83.
[8] 周莉 王鸿博 傅佳佳 陈太球 蒋春燕. 应用电子束辐照技术的棉织物抗菌整理工艺优化[J]. 纺织学报, 2017, 38(10): 81-87.
[9] 吉强 王晓 戚俊然 崔永珠 吕丽华. 光接枝丙烯酸棉纤维素基TiO2/C光催化剂的制备与光催化性[J]. 纺织学报, 2017, 38(10): 75-80.
[10] 张璐璐 丁放 胡雪燕 王鸿博 杜金梅. 疏水图形及面积对棉织物吸湿快干性能的影响[J]. 纺织学报, 2017, 38(09): 89-93.
[11] 解昌峰 刘波 孙建平 唐人成 龙家杰. 活性染料染色棉织物的水溶液浸渍光催化剥色[J]. 纺织学报, 2017, 38(09): 81-88.
[12] 张德锁 陈岭 赵敏 . 改性活性棉织物的纳米银原位组装抗菌整理[J]. 纺织学报, 2017, 38(06): 169-174.
[13] 向中林 韩雪梅 刘增祥 许长海. 棉织物低温酶氧一浴前处理工艺[J]. 纺织学报, 2017, 38(05): 80-85.
[14] 杨书会 王瑞. 纯棉织物折皱回复角与其组织结构参数的关系[J]. 纺织学报, 2017, 38(04): 46-49.
[15] 许云辉 李继丰 王云霞 张飞 杜兆芳. 丝素酰胺改性棉织物的结构及性能[J]. 纺织学报, 2017, 38(02): 134-140.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!