JOURNAL OF TEXTILE RESEARCH ›› 2005, Vol. 26 ›› Issue (1): 73-75.

• 生产技术 • Previous Articles     Next Articles

Preparation of amino-silicone by hydrosilyation reaction

ZHENG Guo;LIU Yan-jun;GE Qi   

  1. Fine-Chemical Institute;Tianjin Polytechnic University;Tianjin 300 160;China
  • Received:1900-01-01 Revised:1900-01-01 Online:2005-02-15 Published:2005-02-15

Abstract: The amino-silicone was prepared by hydrosilylation of hydrogen-silicone with a llyl amino.The amino-value of the amino-sili cone is 0.8~1.5, and then inserted the alkoxy group into the structure to imp rove the crosslink ability.The optimal reactive condition was the toluene as sol vent,H2PtCl6 catalyst content 0.2 mmol/g and added the allyl amino to hyd rogen-silicone dropwise within 2 hours under reflux.Kept the temperature to r ea ct 2~3 h,then added n-propanol containing KOH in 30 minutes and reacted 90 m inutes to gain amino-silicone containing alkoxy group.

No related articles found!
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!