JOURNAL OF TEXTILE RESEARCH ›› 2006, Vol. 27 ›› Issue (1): 68-71.

• 测试分析 • Previous Articles     Next Articles

Pupa protein silk grafted on viscose filament yarn in HIO_3 media

ZHOU Xiao-hua;YANG Liang-zuo;LUO Hui;CHEN Ming-tuo   

  1. Chemistry and Chemical Engineering College;Chongqing University;Chongqing 400044;China
  • Received:2004-12-31 Revised:2005-09-19 Online:2006-01-15 Published:2006-01-15

Abstract: Grafting of pupa protein on oxidative viscose filament yarn was carried out with HIO3at pH value= 5.0,30℃for 2 h.The dosage of HIO3was 0.08 g/g viscose filament yarn.Its grafting percentage was 35.1%.The cross-linking treatment of the grafted silk was conducted with 10% glyoxal at 30℃,pH=4.0 for 3 h,thereby obtained milk white grafted silk with pupa protein content of 5.24% and single fiber breaking strength of 2.9 N,that is only 8% lower than that of viscose filament yarn.No pupa protein released in acetic acid or in NaHCO3solution with pH value= 3.50 or 9.50 respectively.Infrared spectrum analysis showed that the grafted silk has a special absorption of Schiff bases and has a brilliant shade when dyed with methyl red.

No related articles found!